3M Scotchcal™ 3690 Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name ScotchCal™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcal™ 3690 Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some low surface energy materials. Designed with a gray-pigmented adhesive for good hiding power, this permanent film provides long term durability in sever weather and handling conditions encountered by commercial and industrial graphics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
without adhesive
76.2 - 102 microns
3.00 - 4.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 17.2 MPa
>= 2490 psi
Peel Strength 0.526 - 1.05 kN/m
3.00 - 6.00 pli
Adhesion to Powder coat paint
0.877 kN/m
5.00 pli
Adhesion to ABS
0.877 kN/m
5.00 pli
Adhesion to Acrylic enamel
0.877 kN/m
5.00 pli
Adhesion to Aluminum, etched
0.877 kN/m
5.00 pli
Adhesion to Chrome
0.877 kN/m
5.00 pli
Adhesion to Fiberglass
1.05 kN/m
6.00 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 32.0 °C
89.6 °F
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Users viewing this material also viewed the following: