Polymer Property : Peel Strength = 6.00 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri..
Peel Strength 0.526 - 1.05 kN/m
3.00 - 6.00 pli
Adhesion to Powder coat paint
3M Controltac™ 3690C Graphic Film with Comply™ Adhesive
This is a 2-mil white, clear or black film for screen printing graphics. The aggressive, pressure activated-adhesive is slideable and repositionable, and has air release channels for fast and easy b..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ FN180C-10 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
Peel Strength 0.526 - 1.05 kN/m
3.00 - 6.00 pli
Adhesion to Powder coat paint
3M Scotchcal™ 3690 Graphic Film
This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo..
Peel Strength 0.526 - 1.05 kN/m
3.00 - 6.00 pli
Adhesion to Powder coat paint
3M Scotchcal™ 3690LF Graphic Film
This is a 2-mil white for black film for screen printing graphics. The aggressive, pressure sensitive-adhesive is well suited for graphics applied to sand cast, moderately rough surfaces and some lo..
Peel Strength 0.701 - 1.05 kN/m
4.00 - 6.00 pli
Adhesion to Fruehauf pre-painted panel
3M Scotchcal™ IJ780Cv3 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Acrylic
3M Scotchcal™ IJ780Cv3 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-sensitive adhesive with non-visible, air release channels for fast, easy, bubble-free installations; Confirms to flat s..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ 180C Graphic Film with Comply™ Adhesive
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ FN180Cv3-10 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ IJ180-10 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ IJ180C-10 Graphic Film with Comply™ Adhesive
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ IJ180Cv3-10 Graphic Film with Comply™ Adhesive
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ RG180-10 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ RG180C-10 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat..
Peel Strength 0.701 - 1.05 kN/m
4.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Envision™ 480Cv3 Print Wrap Film
High performance, 2-mil white, non-PVC film with a luster finish; Pressure-act adhesive for easy sliding, tacking, snap up and repositioning; non-visible air release channels for fast and easy, bubb..
Peel Strength 0.877 - 1.05 kN/m
5.00 - 6.00 pli
Adhesion to Aluminum, etched
3M Controltac™ 180 Graphic Film
2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri..