Material Notes:
3M Scotchcast Re-enterable Electrical Resin 2123 is a soft, two-part polybutadine resin encapsulant designed especially for re-enterable splice protection. It is formulated for virtually every electrical application requiring a soft, re-enterable resin with good handling and performance characteristics. This resin is also used as the insulating material for cable splicing operating at 1000 volts and is rated for continuous use at 90°C with an overload rating of 130°C. It may be stocked to cover most re-enterable resin needs, ending the need for multiple encapsulant inventories. Scotchcast Resin 2123 is formulated with excellent wetting properties and low viscosity. The resin flows well even at low temperatures, filing the closure and minimizing voids.Information provided by 3M
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.0738 MPa
10.7 psi
ASTM D412
Elongation at Break 300 %
300 %
ASTM D412
Tear Strength 0.280 kN/m
1.60 pli
ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air 90.0 °C
194 °F
Electrical Properties Metric English Comments
Insulation Resistance >= 4.00e+11 ohm
>= 4.00e+11 ohm
MS 17000, Section 1182
Dielectric Constant >= 1.2

@Frequency 100 Hz
>= 1.2

@Frequency 100 Hz
ASTM D150
Dielectric Strength >= 9.45 kV/mm

@Thickness 3.17 mm
>= 240 kV/in

@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.00080

@Frequency 100 Hz
0.00080

@Frequency 100 Hz
ASTM D150
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 21.0 °C
24.0 hour

@Temperature 69.8 °F
Gel Time 62.0 min
62.0 min
Descriptive Properties Value Comments
Appearance Amber Translucent