Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcast™ 3570G-N Connector Sealing Pack

Category Other Engineering Material
Manufacturer 3M
Trade Name Scotchcast™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcast™ 3570G-N Connector Sealing Pack.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The 3M Scotchcast Connector Sealing Pack 3570G-N insulates and provides protection for electrical spring connectors against dust, soil, water, and other environmental elements. Each sealing pack contains a specific amount of the two-part 3M Scotchcast Epoxy Resin 3570G-N in a unique closed mixing pouch. The resin generates its own heat to cure and its compatibility with spring connectors makes this sealing pack a convenient insulating and encapsulating resin for electrical spring connections. The 3570G-N sealing pack will accommodate one 3M Performance plus Wire Connector O/B, R/Y, T/R, T/Y or one 3M Electrical Spring and Grounding Connector 312 or 512.Information provided by 3M
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength at Break 12.3 MPa
1780 psi
ASTM D638
Elongation at Break 57 %
57 %
ASTM D638
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 21.0 °C
69.8 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.2

@Frequency 60.0 Hz,
Temperature 23.0 °C
2.2

@Frequency 60.0 Hz,
Temperature 73.4 °F
ASTM D150
8.9

@Frequency 60.0 Hz,
Temperature 90.0 °C
8.9

@Frequency 60.0 Hz,
Temperature 194 °F
ASTM D150
Dielectric Strength 17.1 kV/mm
435 kV/in
ASTM D149
Processing Properties Metric English Comments
Gel Time 8.00 - 12.0 min
8.00 - 12.0 min
ASTM D24799