3M Scotchkote™ 162PWX Epoxy Coating

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 162PWX Epoxy Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Scotchkote Epoxy Coating 162PWX is a 100% solid two-part epoxy coating that has been specifically developed for the long term protection of drinking water pipelines, storage and process tanks or vessels and related steelwork immersed or in contact with potable water. Scotchkote epoxy coating 162PWX is designed for high build single coat applications by either plural feed hot airless spray equipment, brush or roller.Information provided by 3M
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
Solids Content 100 %
100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Water Absorption 1.05 %
1.05 %
21 days; ASTM D570
Thickness 508 microns
20.0 mil
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
ASTM D2240
Tensile Strength at Break 23.5 MPa
3410 psi
ASTM D638
Elongation at Break 1.4 - 2.0 %
1.4 - 2.0 %
ASTM D638
Flexural Strength 57.00 MPa
8267 psi
ASTM D790
Impact Test 4.50 J
3.32 ft-lb
ASTM G14 (modified)
Abrasion 113
113
[mg] CS-17, 1000 cycles; ASTM D4060
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 50.0 °C
122 °F
71.0 °C
160 °F
onset
Processing Properties Metric English Comments
Cure Time 240 min
4.00 hour
Touch Dry
360 min
6.00 hour
Hard Dry, 1 hr when surface temp at 50°C
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Gray or Blue
Pencil Hardness 5H
ASTM D3363