Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.48 g/cc | 0.0535 lb/in³ | |
Plastcom SLOVAMID 66 GF 30 FRG 5 PA66, 30% glass fibre, flame retarder FeaturesPA 66 for injection moulding, chemically reinforced with 30 % glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 /0,8 mm/ in accordance with .. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
LATI Latan 13 S/15 POM, 15% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
LATI Latilub 66-15T G/30 PA66, 30% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI (Europe-Africa-Middle East) LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer containing PTFE / Silicone. Added features include: Inernally Lubricated |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp RFM62 PA 66 (Asia Pacific) LNP* Lubricomp* RFM62 is a compound based on Nylon 66 resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP JF003E PES (Asia Pacific) LNP* Thermocomp* JF003E is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES LNP* THERMOCOMP* JF003XXZ is a compound based on Polyethersulfone resin containing 15% Glass Fiber. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KFB11 Acetal Copoly LNP* THERMOCOMP* KFB11 is a compound based on Acetal Copolymer resin containing 5% Glass Fiber, 5% Glass Bead. Added features of this material include: Low Warpage, Chemically Coupled. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP MFB429 PP (Asia Pacific) LNP* Thermocomp* MFB429 is a compound based on Polypropylene resin containing Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP SF00A PA12 (Asia Pacific) Glass filled Nylon 12 |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | DIN 53479 |
Polyram PA310G8 Nylon 66, 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183-87 |
Wellman Wellamid® FRGF25-66 NBK3 Nylon 66, 25% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183-87 |
Wellman Wellamid® MRGF25/15 42H-WBK Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced, Weatherable Grade BlackAll information provided by Wellman Engineered Resins. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® XT-5038-9 Two-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
CP-Polymer-Technik Wellamid® 6600 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Density | 1.48 g/cc @Temperature 23.0 °C |
0.0535 lb/in³ @Temperature 73.4 °F |
DIN 53 479 |
Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D1505 |
DuPont Teijin Films Melinex® 331 Polyester Film, 700 Gauge Melinex® 331 is an opaque, pearlescent, white film with excellent handling properties that is pretreated on one side to promote adhesion to most industrial coatings.Approvals: UL Recognition - Prod.. |
|||
Density | 1.48 - 1.52 g/cc | 0.0535 - 0.0549 lb/in³ | ISO 1183 |
Fainplast Compounds Hax™ HFX 505 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
Arkema Group Nakan® FKS 918 R PVC, Soft Extrusion Grade NAKAN FKS 918 R is a soft polyvinyl chloride compound developed for general insulation and sheathing.ISO data provided by the manufacturer, Arkema. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 183 |
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Conditioned, 40% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
BASF Ultramid® SEGM35 H1 BK 6259 40% Glass/Mineral Filled PA6 (Conditioned) Description: Ultramid SEGM35 H1 BK6259 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compar.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | |
A. Schulman ComAlloy Hiloy® 629 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics SABIC STAMAX 60YM240 PP SABIC® STAMAX 60YM240 is a 60% long glass fiber reinforced polypropylene concentrate, specially developed for dilution with SABIC®PP homopolymer. The glass fibers are chemically couplied to the PP.. |
|||
Density | 1.48 g/cc | 0.0535 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard.. |