3M Scotchkote™ CR 511 Epoxy Ceramic Surface

Category Polymer , Thermoset , Epoxy
Manufacturer 3M
Trade Name Scotchkote™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ CR 511 Epoxy Ceramic Surface.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Epoxy Ceramic CR 511 has been specifically developed as a 100% solids coating for resurfacing and lining to improve the efficiency of equipment in fluid flow environments.Product Features:Combines good application characteristics with good erosion and corrosion resistanceDesigned for application by brushProvides a low friction surface improving flow rates in pumps, etc.Designed for resurfacing and lining metal components. Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Thickness 254 microns
10.0 mil
Mechanical Properties Metric English Comments
Flexural Strength 55.8 MPa
8100 psi
Compressive Strength 68.9 MPa
10000 psi
Shear Strength 17.2 MPa
2500 psi
Tensile Shear Adhesion
Abrasion 0.080
0.080
[g] 1 kg, CS17; ASTM D4060
Processing Properties Metric English Comments
Cure Time 360 min
6.00 hour
Touch Dry
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Light Gray, Blue and Red