Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ASTM D2240
Tensile Strength, Ultimate 41.4 MPa
6000 psi
ASTM D412
Tensile Strength, Yield 4.83 MPa
700 psi
at 100%; ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
Tear Strength 87.7 kN/m
500 pli
die B; ASTM D624
Compression Set 16 %
16 %
ASTM D395