A. Schulman ComAlloy Aqualoy® 150 Polypropylene, Glass Reinforced, Chemically Coupled NSF

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer A. Schulman ComAlloy
Trade Name Aqualoy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Aqualoy® 150 Polypropylene, Glass Reinforced, Chemically Coupled NSF.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability and high strength traits into a unique property blend.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Ultimate 107 MPa
15500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 153 MPa
22200 psi
ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.99 J/cm
13.1 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
327 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 229 - 246 °C
444 - 475 °F