Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Comtuf® 102 Polypropylene, Mineral Reinforced, Impact Modified

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced, Impact Modified
Manufacturer A. Schulman ComAlloy
Trade Name COMTUF®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Comtuf® 102 Polypropylene, Mineral Reinforced, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Ultimate 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 289 %
289 %
ASTM D638
Flexural Strength 34.0 MPa
4930 psi
ASTM D790
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.3 J/cm
19.3 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
180 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Users viewing this material also viewed the following: