Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Voloy® 413 Polyester - PBT, Glass Reinforced, Flame Retardant, UL

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer A. Schulman ComAlloy
Trade Name Voloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Voloy® 413 Polyester - PBT, Glass Reinforced, Flame Retardant, UL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.70 g/cc
0.0614 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Ultimate 125 MPa
18100 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Flexural Strength 175 MPa
25400 psi
ASTM D790
Flexural Modulus 10.2 GPa
1480 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.00 J/cm
7.49 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 - 225 °C
410 - 437 °F
Deflection Temperature at 0.46 MPa (66 psi) 223 °C
433 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
397 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 235 - 249 °C
455 - 480 °F