Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0060 in/in

@Thickness 0.126 in
72 hr; ISO 294
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
15 sec delay; ISO 868
Tensile Strength, Ultimate 15.0 MPa
2180 psi
at max load; ISO 527
Elongation at Break 150 %
150 %
ISO 527
Flexural Modulus 0.911 GPa
132 ksi
Tangent; ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 63.0 °C

@Thickness 3.20 mm
145 °F

@Thickness 0.126 in
ISO 75