Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Glass/Mineral Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ash 35 %
35 %
ASTM D2584
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.0 MPa
9140 psi
50 mm/min; ASTM D638
Flexural Modulus 4.60 GPa
667 ksi
ASTM D790
Izod Impact, Notched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
289 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ASTM D648