Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.600 - 1.30 J/cm @Temperature -30.0 - 0.000 °C |
1.12 - 2.44 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.875 J/cm Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.600 - 1.30 J/cm @Thickness 3.17 - 3.17 mm |
1.12 - 2.44 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.875 J/cm Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATAN 23 Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Izod Impact, Notched | 0.600 - 1.12 J/cm @Temperature -30.0 - -30.0 °C |
1.12 - 2.10 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.864 J/cm Grade Count:9 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
1.12 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | Molded; ASTM D256 |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | Molded; ASTM D256 |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | 23° C; ASTM D256 |
Flint Hills PP 13R9A Random Copolymer Polypropylene Random copolymer, Drug Master File (DMF) listed, USP Class VI certified, and FDA compliantFeatures: Radiation resistant and good contact clarity.Applications: Injection molding: radiation sterilizab.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
Loxim 220 01HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 815 PBT (Europe-Africa-Middle East) VALOX 815 is a 15% glass reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housings assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SPS Guang Zhou POBUXâ„¢ 3001EPG15 Non-halogen flame retardance/GF15%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 3.20 mm |
1.12 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6411 1924 Light Stabilized Polystyrene Characteristics Prevents dust patterns due to static charges High gloss Good flow Improved light fastness Processing Injection molding Extrusion Applications A/C and cooler grill Material Status.. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
UBE UBESTA® 3020X25L Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for coating steel and aluminumInformation provided by UBE. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM-D256 |
Toyobo VYLOPET® EMC320R Polyester Resin VYLOPET® is a polyester resin developed specifically for injection molding. Polyester resins have excellent heat resistance, rigidity, chemical resistance, and electric properties. Grade EMC320R ha.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM1419 Acetal, PTFE Filled Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.600 - 0.800 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.12 - 1.50 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass Characteristics: 30% glass fibre filled |
|||
Izod Impact, Notched | 0.600 - 0.700 J/cm | 1.12 - 1.31 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color.. |
|||
Izod Impact, Notched | 0.598 J/cm | 1.12 ft-lb/in | ASTM D256 |
Cheng Yu Plastic A707G2 SAN, 20% Glass Fiber |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1943 CaC03 and Glass Fiber Hybrid Copolymer Polypropylene DescriptionPolyfort® FXP 1943 is a 20% CAC03 and glass fiber hybrid copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.600 J/cm | 1.12 ft-lb/in | ISO 180 |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |