A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer A. Schulman, Inc.
Trade Name POLYFORT™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.892 - 0.916 g/cc
0.892 - 0.916 g/cc
ASTM D792
Melt Flow 30 - 36 g/10 min

@Temperature 230 °C
30 - 36 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Flexural Modulus 0.930 GPa
135 ksi
ASTM D790
Falling Dart Impact 2.26 J
1.67 ft-lb
-30°C (colors); GM9300P
20.00 J
14.75 ft-lb
-30°C (natural); GM9300P
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Descriptive Properties Value Comments
Thermal Oxidative Stability 336 hours
ASTM D3012
Users viewing this material also viewed the following: