Material Notes:
DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Index of Compound 8.0 g/10 min
8.0 g/10 min
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
at max load; ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Gardner Impact 15.02 J
11.08 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648