Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | Tangent; ASTM D790 |
NOVA Chemicals Novapol® HE-Y449-A HDPE Extrusion Resin Features: High ESCR, good toughness, good chemical resistance, good processability.Applications: Pipe coatings, profile extrusions, sheet extrusion for thermoforming, corrugated tubing, conduit.Data.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Petromont 4102 High Density Polyethylene Resin Petromont HDPE 4102 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is intended for general use in large diameter light weight drainage tubing applicat.. |
|||
Flexural Modulus | 1.14 - 5.10 GPa | 165 - 740 ksi | Average value: 2.06 GPa Grade Count:118 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | at 0.05 in/min; ASTM D790 |
M. Holland Company CP400 Polypropylene Copolymer Features: Medium Flow, High Impact ResistanceUses: Appliances, Business Equipment, Construction Applications, Tool/Tote Box, ToysProcessing Method: Injection MoldingInformation provided by M. Hollan.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Kostat ICP-STAT ICS-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Laurel BioComposite Bio-Resâ„¢ 20% Composite in HDPE Bio-Resâ„¢ can be blended with various resins in certain applications. It can be included at rates up to 40% in manufactured plastic products while maintaining or enhancing the desired characteri.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Kostat ICP-STAT ICD-1002 PP Sheet KOSTATs ICP-STAT is a thermoplastic sheet coated with an inherently conductive polymer (ICP). ICP-STAT has distinctive advantages in ESD and cleanliness performances compared to other materials bas.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Techmer ES Electrablend® ABS 03106 MB Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech Soft Touch HDPE Polyolefin Skin/Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
Spartech SP-1510 Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1259 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1259 is a medium impact polypropylene with easier molding characteristics for thinner parts and longer flow distances. Lower molding pressures and heats often reduce war.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 0.05 in/min; ASTM D790 |
A. Schulman PP 1579 Polypropylene Impact Grade Polypropylene DescriptionPolypropylene PP 1579 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided by A.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | tangent; ASTM D790 |
A. Schulman LB502-01 High Molecular Weight, High-Density Polyethylene Copolymer DescriptionLP 502-01 Natural is a high molecular weight, high-density polyethylene copolymer, designed for blow molding of large parts where the finished product demands outstanding physical perform.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | ASTM D790 |
A. Schulman PP 1452 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1452 is a medium impact polypropylene with a good balance of stiffness and impact resistance. It is stabilized for heat stability, and is chemical resistant.Information .. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6510A Injection Molding Polypropylene Impact CopolymerApplications: Closures, Housewares, Small Appliance, Battery Cases and LidsFormolene 6510A is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6520A Injection Molding Polypropylene Impact CopolymerApplications: Closures, Housewares, Small Appliance ApplicationsFormolene 6520A is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property b.. |
|||
Flexural Modulus | 1.14 GPa | 165 ksi | |
CMW® ELKONITE® 40W3 Infiltrated Tungsten Copper material ASTM B702 For vacuum switch contacts, low expansion structural members.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.14 - 6.21 GPa | 165 - 900 ksi | Average value: 3.16 GPa Grade Count:42 |