Material Notes:
ACP 5080 is a 5xxx series precision aluminum cast plate. Thickness, flatness and surface finish offer very tight tolerances.Material stability and excellent processing characteristics make this aluminum alloy the right choice for fixtures, tools and general applications Information provided by ALIMEX GmbHHomogenized and stress relieved
Physical Properties Metric English Comments
Density 2.66 g/cc
0.0960 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 70
70
Tensile Strength, Ultimate 290 MPa
42100 psi
Rm
Tensile Strength, Yield 130 MPa

@Strain 0.200 %
18900 psi

@Strain 0.200 %
Elongation at Break 16 %
16 %
Modulus of Elasticity 70.0 GPa
10200 ksi
Thermal Properties Metric English Comments
CTE, linear 24.3 µm/m-°C

@Temperature 20.0 °C
13.5 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 109 - 140 W/m-K
756 - 972 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000004914 ohm-cm
0.000004914 ohm-cm