ATI Allegheny Ludlum AL 45™ Magnetic Alloy

Category Metal , Electronic/Magnetic Alloy , Ferrous Metal
Manufacturer ATI Allegheny Ludlum
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allegheny Ludlum AL 45™ Magnetic Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in sheet and strip for use in relays, rotors, stators, glass-to-metal seals. ASTM A753 Type 1Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Iron, Fe 55 %
55 %
as balance
Nickel, Ni 45 %
45 %