Material Notes:
Slightly higher wear resistance and lower toughness than M2. Typical application similar to that of M2.Information provided by Allegheny Ludlum
Component Elements Properties Metric English Comments
Carbon, C 1.07 %
1.07 %
Chromium, Cr 4.0 %
4.0 %
Iron, Fe 82 %
82 %
as balance
Molybdenum, Mo 5.1 %
5.1 %
Tungsten, W 5.5 %
5.5 %
Vanadium, V 2.4 %
2.4 %