Material Notes:
Silicon and iron alloyApplications:relays, armatures, solenoids, magnetic clutches, pole pieces, certain types of motors, transformers, data processing equipment.Information provided by Allegheny Ludlum
Physical Properties Metric English Comments
Specific Gravity 7.75 g/cc
7.75 g/cc
Assumed for magnetic purposes per ASTM test specifications
Density 7.723 g/cc
0.2790 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 65 - 80
65 - 80
Tensile Strength, Ultimate 455.1 MPa
66010 psi
Tensile Strength, Yield 330.9 MPa

@Strain 0.200 %
47990 psi

@Strain 0.200 %
Elongation at Break 31 %
31 %
in 2"
Component Elements Properties Metric English Comments
Aluminum, Al 0.25 %
0.25 %
Silicon, Si 1.25 %
1.25 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000300 ohm-cm
0.0000300 ohm-cm
Magnetic Coercive Force, Hc 0.44 Oe
0.44 Oe
1550°F, 4 hours, Wet Forming Gas
Magnetic Saturation Flux Density, Bmax 20600 Gauss
20600 Gauss
Saturation Induction
Magnetic Remanence, Br 10300 Gauss
10300 Gauss
1550°F, 4 hours, Wet Forming Gas
Curie Temperature 760 °C
1400 °F