Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROLENE® AVPS GPPS 100-1 Clear, Virgin Polystyrene Resin

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Transparent Grade
Manufacturer Aaron Industries Corporation
Trade Name AAROLENE® AVPS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROLENE® AVPS GPPS 100-1 Clear, Virgin Polystyrene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose polystyrene resin, specifically designed for all injection molding applications.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.5 MPa
6600 psi
ASTM D638
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Users viewing this material also viewed the following: