Abatron AboCast 50-11/AboCure 50-1 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 50-11/AboCure 50-1 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 240 min. at 25°C(77°F). Exothermic Peak 190°C (375°F). Hardens in 2-24 hours at RT (faster with heat). Full cure in 1-5 weeks at RT or 1-4 hrs at 80-120°C (175-250°F).
Physical Properties Metric English Comments
Viscosity Measurement 2300
2300
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
Tensile Strength, Ultimate 54.33 MPa
7880 psi
Elongation at Break 14.4 %
14.4 %
Flexural Yield Strength 78.81 MPa
11430 psi
Flexural Modulus 1.58 GPa
229 ksi
Compressive Yield Strength 71.02 MPa
10300 psi
Compressive Modulus 1.65 GPa
239 ksi
Izod Impact, Notched 0.235 J/cm
0.440 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 2.42e+15 ohm-cm
2.42e+15 ohm-cm
Surface Resistance 7.85e+15 ohm
7.85e+15 ohm
Dielectric Constant 2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
3.06

@Frequency 1000 Hz
3.06

@Frequency 1000 Hz
3.09

@Frequency 60 Hz
3.09

@Frequency 60 Hz
Dissipation Factor 0.0078

@Frequency 1000 Hz
0.0078

@Frequency 1000 Hz
0.0089

@Frequency 60 Hz
0.0089

@Frequency 60 Hz
0.017

@Frequency 1e+6 Hz
0.017

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 240 min
240 min
500 g
Descriptive Properties Value Comments
Exotherm 190°C
Peak