Abatron AboCast 8-4/Abocure 8-4 Epoxy  (discontinued **)

Category Polymer , Thermoset , Epoxy
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8-4/Abocure 8-4 Epoxy  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2-part solvent-free dielectric epoxy casting compound.Processing: 100/60 ratio (pbw); Gel time, 100 g (3.5 oz.): 240 minutes; cures in 3 weeks at 25°C (77°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.26 %
0.26 %
in 24 hours.
Viscosity Measurement 1200
1200
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
Tensile Strength, Ultimate 50.33 MPa
7300 psi
Elongation at Break 4.5 %
4.5 %
Flexural Strength 93.77 MPa
13600 psi
Electrical Properties Metric English Comments
Electrical Resistivity 8.00e+10 ohm-cm

@Temperature 93.3 °C
8.00e+10 ohm-cm

@Temperature 200 °F
5.00e+12 ohm-cm

@Temperature 65.6 °C
5.00e+12 ohm-cm

@Temperature 150 °F
4.00e+15 ohm-cm

@Temperature 25.0 °C
4.00e+15 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 3.36

@Frequency 1e+6 Hz
3.36

@Frequency 1e+6 Hz
Dissipation Factor 0.013

@Frequency 1e+6 Hz
0.013

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 3 weeks