Abatron AboCast 8503-7/AboCure 8503-7 Colorless Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 8503-7/AboCure 8503-7 Colorless Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 8503-7/AboCure 8503-7 is a general purpose, slow hardening, colorless epoxy casting compound with low viscosity. It is similar to the 8503-4 system, but more flexible. Suggested Uses: Transparent Casting, Embedding, Encapsulation, Potting, and Bonding. Casting display or experimental models without the high shrinkage of acrylic or other resins. Precise reproduction of anatomical or scientific models. Embedding organic, geologic, or metallurgic specimens. Encapsulation of electric, radioactive, or delicate components. Preservation or repair of artistic and historical objects. High-performance transparent table tops.
Physical Properties Metric English Comments
Viscosity 700 cP
700 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
Tensile Strength at Break 51.7 MPa
7500 psi
Elongation at Break 17 %
17 %
Flexural Strength 69.6 MPa
10100 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 45.0 °C
113 °F
Deflection Temp at unknown load
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Pot Life 90 min

@Temperature 25.0 °C
90 min

@Temperature 77.0 °F
500 g
Descriptive Properties Value Comments
Hardening Time (min) 120-720
Parts by Weight (pbw) 100
AboCast
60
AboCure