Aclo Accucomp ABS ABS811L Medium Impact Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Aclo Compounders
Trade Name Accucomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accucomp ABS ABS811L Medium Impact Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
MD; ASTM D955
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.0 MPa
6670 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Tensile Modulus 1.750 GPa
253.8 ksi
ASTM D638
Flexural Strength 69.98 MPa
10150 psi
ASTM D790
Flexural Modulus 2.699 GPa
391.5 ksi
ASTM D790
Izod Impact, Notched 3.74 J/cm
7.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 83.9 °C
183 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
163 °F