Aclo Accutech Polycarbonate POL051G40L Glass Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 40% Glass Filled
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polycarbonate POL051G40L Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
MD; ASTM D955
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 114
114
ASTM D785
Tensile Strength at Break 141.0 MPa
20450 psi
ASTM D638
Tensile Strength, Yield 142.0 MPa
20590 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 5.799 GPa
841.1 ksi
ASTM D638
Flexural Strength 215.9 MPa
31320 psi
ASTM D790
Flexural Modulus 10.998 GPa
1595.1 ksi
ASTM D790
Izod Impact, Notched 1.82 J/cm
3.40 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 144 °C
291 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
Users viewing this material also viewed the following: