Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 6.35 mm |
291 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Lexan® 3414R PC (Europe-Africa-Middle East) LEXAN 3414R is a high viscosity, 40% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East) Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Lexan® XHT1141 PC XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1200-08 Polycarbonate Resin Description: LUPOY PC 1200-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 3030-10 Polycarbonate Resin Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 4.00 mm |
291 °F @Thickness 0.157 in |
Annealed; ASTM D648 |
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP LUBRICOMP PL002 PA 6 LNP* LUBRICOMP* PL002 is a compound based on Nylon 6 base resin containing 10% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 IM 40 Z Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer (Europe-Africa-Middle East) Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity... |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing 15% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOCOMP DF003E PC (Asia Pacific) LNP* Thermocomp* DF003E is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | annealed; ASTM D648 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B |
Styron CALIBREâ„¢ 201-10 Polycarbonate Resin Overview: CALIBREâ„¢ 201-10 is produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. It provides excellent impact resistance, heat distortion resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | annealed; ASTM D648 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Samyang Trirex® 3020A Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020A is a high flow grade with heat stabilizers.Information provided by Samyang. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Samyang Trirex® 3020PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020PJ is a high flow grade.Information provided by Samyang. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Samyang Trirex® 3020U UV Stable Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020U is a high flow, UV Stable grade.Information provided by Samyang. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C @Thickness 3.20 mm |
291 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP DF004 PC LNP* THERMOCOMP* DF004 is a compound based on Polycarbonate resin containing 20% Glass Fiber. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B; ASTM D648 |
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Annealed; ISO 75-2/B |
Styron CALIBREâ„¢ 701-10 Polycarbonate Resin Overview: CALIBREâ„¢ 701-10 resin is formulated and produced to supply clarity and enhanced ignition resistance. They do so while maintaining excellent physical properties and processability. CAL.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp XF006S LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Aclo Accutech Polycarbonate POL051G10L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Aclo Accutech Polycarbonate POL051G30L Glass Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | ASTM D648 |
Ashley Polymers Ashlene® P265 PPO, 20% Glass Reinforced A general purpose, 20% glass reinforced PPO resin for injection molding applications requiring structural strength, dimensional stability and good heat resistance.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |