Aclo Accutech Polypropylene Copolymer CP0436M10L Mica Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 10% Mica Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0436M10L Mica Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 10 %
10 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 53
53
ASTM D785
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 26 %
26 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 1.500 GPa
217.5 ksi
ASTM D638
Flexural Strength 27.0 MPa
3920 psi
ASTM D790
Flexural Modulus 1.350 GPa
195.8 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F