Material Notes:
Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Conditioned; ISO 868
84
84
ISO 868
Tensile Strength at Break 80.0 MPa
11600 psi
Conditioned; ISO R 527
120 MPa
17400 psi
ISO R 527
Elongation at Yield 5.0 %
5.0 %
ISO R 527
7.0 %
7.0 %
Conditioned; ISO R 527
Modulus of Elasticity 3.50 GPa
508 ksi
Conditioned; ISO 178
6.00 GPa
870 ksi
ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
ISO 180/1A
16.0 kJ/m²
7.61 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
ISO 179/IeU
5.50 J/cm²
26.2 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
ISO 179/IeA
1.20 J/cm²
5.71 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
ASTM E831
Melting Point 220 °C
428 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-2/AF
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Conditioned; CEI 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
CEI 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
Conditioned; CEI 60243-1
33.0 kV/mm
838 kV/in
CEI 60243-1
Comparative Tracking Index 550 V
550 V
CEI 60112/Solution A