Advanced Ceramics MEXIM C ACL 2091

Category Ceramic , Glass , Glass Ceramic
Manufacturer Advanced Ceramics Limited
Trade Name MEXIM C
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Ceramics MEXIM C ACL 2091.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mexim C has been specially formulated to give an expansion closely matched to that of copper. It has high electrical insulation properties and good mechanical strength, and finds increasing application as a conformal insulating layer on copper substrates as well as conventional electrical lead-throughs.Information provided by Advanced Ceramics Limited (ACL)
Physical Properties Metric English Comments
Density 3.142 g/cc
0.1135 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.250 GPa

@Temperature 20.0 °C
36.3 ksi

@Temperature 68.0 °F
Thermal Properties Metric English Comments
CTE, linear 16.5 - 17.7 µm/m-°C

@Temperature 20.0 - 700 °C
9.17 - 9.83 µin/in-°F

@Temperature 68.0 - 1290 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm

@Temperature 300 °C
1.00e+12 ohm-cm

@Temperature 572 °F
1.90e+17 ohm-cm

@Temperature 20.0 °C
1.90e+17 ohm-cm

@Temperature 68.0 °F
Dielectric Constant 5.8

@Frequency 10000 Hz
5.8

@Frequency 10000 Hz
5.8

@Frequency 1e+8 Hz
5.8

@Frequency 1e+8 Hz
6.2

@Frequency 3.00e+9 Hz
6.2

@Frequency 3.00e+9 Hz
Dielectric Strength 28.0 kV/mm
711 kV/in
Breakdown
Dissipation Factor 0.00020

@Frequency 1e+8 Hz
0.00020

@Frequency 1e+8 Hz
0.00085

@Frequency 10000 Hz
0.00085

@Frequency 10000 Hz
0.00265

@Frequency 3.00e+9 Hz
0.00265

@Frequency 3.00e+9 Hz