Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 23.0 °C |
1.00e+12 ohm-cm @Temperature 73.4 °F |
50%RH; ASTM D257 |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Zytel® 105F BK010 is a lubricated, fast cycling, weather resistant PA 66 resin. Zytel® 105F BK010 contains finely dispersed carbon black.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 150 °C |
1.00e+12 ohm-cm @Temperature 302 °F |
DC; DIN 40634 or VDE 0345 in air or ASTM D257 |
Mitsubishi Hostaphan® WN, 190 micron Nominal Thickness Translucent White Polyethylene Terephthalate Film Hostaphan® WN is a white film made of polyethylene terephthalate (PET) and is well suited for electrical insulating of machines and appliances. The high dielectric strength and large volume resis.. |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 100 °C |
>= 1.00e+12 ohm-cm @Temperature 212 °F |
|
Master Bond EP112LS Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation Master Bond EP112LS is a low viscosity two component epoxy resin system for potting, encapsulation, sealing, coating and impregnation. The mix ratio is an easy to use 100:80 by weight. EP112LS offer.. |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 400 °C |
>= 1.00e+12 ohm-cm @Temperature 752 °F |
|
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 400 °C |
>= 1.00e+12 ohm-cm @Temperature 752 °F |
|
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation pr.. |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 200 °C |
1.00e+12 ohm-cm @Temperature 392 °F |
ASTM-D257 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 200 °C |
1.00e+12 ohm-cm @Temperature 392 °F |
ASTM-D257 |
CeramTec Rubalit® 708 Alumina, 96% Based on 96% aluminum oxide, Rubalit® 708 was developed specifically for making heavy-duty resistors and miniature metal layer resistors. Because of its outstanding strength, this same material is .. |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 500 °C |
1.00e+12 ohm-cm @Temperature 932 °F |
|
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 400 °C |
>= 1.00e+12 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec Rubalit® A 1999.5 Alumina, 99.7% Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat.. |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 100 °C |
1.00e+12 ohm-cm @Temperature 212 °F |
IEC 672-1 |
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 100 °C |
1.00e+12 ohm-cm @Temperature 212 °F |
IEC 672-1 |
CeramTec Sikor® S Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 25.0 °C |
>= 1.00e+12 ohm-cm @Temperature 77.0 °F |
|
Master Bond EP40 High Shear and Peel Strength, Two Component, Flexible Epoxy Master Bond Polymer System EP40 is newly developed two component highly flexible epoxy compound for high performance bonding, potting, encapsulation, and sealing with outstanding shear and peel stre.. |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 25.0 °C |
>= 1.00e+12 ohm-cm @Temperature 77.0 °F |
ASTM-D257 |
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 300 °C |
1.00e+12 ohm-cm @Temperature 572 °F |
ASTM-D1829 |
CoorsTek ADS-96R 96% Alumina Thick Film Substrate This high-purity material ensures strong, reliable performance for ceramic substrate application. Applications: thick films and lasers |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 300 °C |
>= 1.00e+12 ohm-cm @Temperature 572 °F |
ASTM-D257 |
CoorsTek ADS-995 99.5% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 300 °C |
>= 1.00e+12 ohm-cm @Temperature 572 °F |
ASTM-D257 |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | >= 1.00e+12 ohm-cm @Temperature 500 °C |
>= 1.00e+12 ohm-cm @Temperature 932 °F |
ASTM-D257 |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 23.0 °C |
1.00e+12 ohm-cm @Temperature 73.4 °F |
50%RH; IEC 60093 |
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6
(Unverified Data**) Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 23.0 °C |
1.00e+12 ohm-cm @Temperature 73.4 °F |
50%RH; ASTM D257 |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 300 °C |
1.00e+12 ohm-cm @Temperature 572 °F |
|
Advanced Ceramics MEXIM C ACL 2091 Mexim C has been specially formulated to give an expansion closely matched to that of copper. It has high electrical insulation properties and good mechanical strength, and finds increasing applicat.. |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 23.0 °C |
1.00e+12 ohm-cm @Temperature 73.4 °F |
50%RH; ASTM D257 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) Zytel® 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 200 °C |
1.00e+12 ohm-cm @Temperature 392 °F |
ASTM-D257 |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
Volume Resistivity | 1.00e+12 ohm-cm @Temperature 200 °C |
1.00e+12 ohm-cm @Temperature 392 °F |
IEC 345 |
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance) Rubalit® 708 HP (High Performance) has been developed from Rubalit® 708S. This material shares the same chemical composition, is produced on the same plant and using the identical production techn.. |