Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Conditioned, 50% Glass Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer Akro-Plastic
Trade Name Akromid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Conditioned, 50% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Nevertheless, the viscosity features are on the level of PA6. Especially after storage, e.g. at 150° AKROMID RM shows comparable ageing characteristics. For appliances with very constant features, low warpage, very good finish together with an improved chemical resistance and for production of parts according to the GIT/WIT process, the version B3 GF 30 RM 9 black (3099) or respectively B3 GF 50 9 RM black (3147) offers an ideal solution. However, if a very good impact strength is predominant, our type B3 GF 30 RM black (3016) or respectively B3 GF 50 RM black (3146) will be favored.High quality surface finish:B3 GF 30 9 RM black (3099)/B3 GF 50 9 RM black (3147)Very constant features with regard to climateVery low warpageVery good surfaceCaCI2 resistantCost-effective:B3 GF 30 RM black (3016)/B3 GF 50 RM black (3146)Closer to PA 6 GF 30/GF 50Constant features with regard to climateLow warpageTendentious higher impact strengthTendentious higher notched impactApplications:Electronic market:e.g. sensor housings, coil former (wo.UL), plug-in connectors, plug panels etc.Automobile market:e.g. sensor housing, electrical parts, wind screen wiper bows, door handles, mirror elements, sliding roof frames etc.General mechanical engineering:e.g. control elements in printer, copier, housings of valves, pumps etc.Information from Akro-Plastic
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ISO 1183
Filler Content 50 %
50 %
ISO 1172
Water Absorption 1.2 %

@Temperature 70.0 °C
1.2 %

@Temperature 158 °F
62% RH, Humidity; ISO 1110
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
5 [mm/min]; ISO 527-2/5
Elongation at Break 3.0 %
3.0 %
5 [mm/min]; ISO 527-2/5
Tensile Modulus 13.0 GPa
1890 ksi
1 [mm/min]; ISO 527-2/1
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
7.00 J/cm²

@Temperature 23.0 °C
33.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ISO 11357-1