Material Notes:
CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and tints availableCorona treatment availableMatte and gloss available3 strategic manufacturing locationsPropertiesExcellent clarity and stiffnessSuperb yieldSuperior dimensional stabilityExcellent ink adhesionIdeal for metallizing applicationsFDA compliant to CFR #177.1640Kosher materialInformation provided by Alcoa Kama Co.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Thickness 25.4 - 102 microns
1.00 - 4.00 mil
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.2 - 82.7 MPa
8000 - 12000 psi
ASTM D638
Elongation at Break 3.0 - 10 %
3.0 - 10 %
ASTM D638
Tensile Modulus 2.76 - 3.10 GPa
400 - 450 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 79.4 °C
175 °F
Minimum Service Temperature, Air -17.8 °C
0.000 °F
Descriptive Properties Value Comments
Resistance to Acid Good to Excellent
Resistance to Alcohols Good to Excellent
Resistance to Alkalis Excellent
Resistance to Fat, Grease, and Oil Good
Resistance to Hydrocarbon Solvents Poor
Resistance to Strong Oxidizers Poor
Yield, in²/lb/mil 26360