AlphaGary AlphaSeal™ 388 D Polyolefin Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer AlphaGary
Trade Name AlphaSeal™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary AlphaSeal™ 388 D Polyolefin Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AlphaSeal™ 388 D is a polyolefin/TPE material recommended for a liner in wine bottle caps. AlphaSeal is formulated for low taste and low odor and exhibits good elastic recovery, abrasion resistance and low temperature behavior. This material is made to tight, exacting specifications.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
Tensile Strength 4.14 MPa
600 psi
Elongation at Break 120 %
120 %