Mechanical Properties Metric English Comments
Tensile Strength >= 4.14 MPa
>= 600 psi
ASTM D412
Parker Chomerics CHO-SEAL® 0862 Conductive Elastomer
Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Extruded onlyRoHS CompliantInformation provided by Chomerics
Tensile Strength 4.14 MPa
600 psi
ASTM D412
Parker Chomerics Waveguide Gaskets 877 Conductive Silicone Elastomer Gasket
Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W..
Tensile Strength 4.14 MPa

@Strain 100 %
600 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible SL60 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 4.14 MPa

@Strain 100 %
600 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 4.14 MPa

@Strain 100 %
600 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R5160A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 4.14 MPa
600 psi
ASTM F152
Garlock GRAPH-LOCK® 3123/3125 Graphite Sheet Gasketing
A pure graphite sheet. Thicknesses
Tensile Strength 4.14 MPa
600 psi
Typical properties on film cast from toluene solution; ASTM D412
Kraton® D1113 P (SIS) Linear Block Copolymer
Description: Kraton D1113 P is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 16%. It is supplied from North America in the physical form identified: Kra..
Tensile Strength >= 4.14 MPa
>= 600 psi
BAM 1211
Kraton® G4609 H (SEBS) with Oil
Description: Kraton G4609 H is a white mineral oil extended linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. Nominal oil content of the polymer is ..
Tensile Strength 4.14 MPa
600 psi
ASTM D412
Kraton® G7705 GI-B (SEBS) Compound
Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Tensile Strength 4.14 MPa
600 psi
ASTM D412
Kraton® G7705 GI-N (SEBS) Compound
Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..
Tensile Strength 4.14 MPa
600 psi
Teknor Apex Elexar® EL 3954-50 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Tensile Strength >= 4.14 MPa
>= 600 psi
Compound Property
Arlon 51393R031 0.031 (0.635 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: 150 Cycles (temperature and time dependent)This data represents typical values for the production material. T..
Tensile Strength 4.14 MPa
600 psi
Silicone Property; ASTM D412
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re..
Tensile Strength 4.14 MPa
600 psi
AlphaGary AlphaSeal™ 388 D Polyolefin Thermoplastic Elastomer
AlphaSeal™ 388 D is a polyolefin/TPE material recommended for a liner in wine bottle caps. AlphaSeal is formulated for low taste and low odor and exhibits good elastic recovery, abrasion resistanc..