Material Notes:
75°C or 80°C low temperature rated flexible jacketing compound intended for UL 62 application
Mechanical Properties Metric English Comments
Tensile Strength 15.2 MPa
2200 psi
Elongation at Break 300 %
300 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -30.0 °C
-22.0 °F
Oxygen Index 26 %
26 %