Polymer Property : Tensile Strength = 15.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 15.2 MPa

@Temperature 136 °C,
Time 605000 sec
2200 psi

@Temperature 277 °F,
Time 168 hour
Air Oven Aged
S&E Specialty Polymers TufFlex™ GA-5330D PVC/PU Compound
Application: 105°C, matte finish, flame retardant PVC/PU jacketing material designed for retractile cord applications.Information provided by S&E Specialty Polymers
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
S&E Specialty Polymers TufTech™ G-2175A PVC Compound
Application: A clear, high gloss, PVC based compound designed for profile extrusion applications.Information provided by S&E Specialty Polymers
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
S&E Specialty Polymers TufTech™ G-3468-A PVC Compound
Application: A general purpose PVC based extrusion grade compound.Information provided by S&E Specialty Polymers
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
S&E Specialty Polymers TufTech™ GA-8705-03 Natural Gloss PVC Compound
Application: 75°C lead free, RoHS compliant riser jacketing compound.Information provided by S&E Specialty Polymers
Tensile Strength 15.2 MPa

@Strain 100 %
2200 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A4D02 Polyvinyl Chloride, Flexible (PVC, Flexible)
A flexible transparent PVC Compound designed primarily for indoor mats.Information provided by PolyOne
Tensile Strength 15.2 MPa

@Strain 100 %
2200 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A5D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tensile Strength 15.2 MPa

@Strain 100 %
2200 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A5DU0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tensile Strength 15.2 MPa

@Strain 100 %
2200 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A5DUB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 15.2 MPa

@Strain 100 %
2200 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3437 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Tensile Strength 15.2 MPa

@Strain 100 %
2200 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3784 Polyvinyl Chloride, Flexible (PVC, Flexible)
All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high ..
Tensile Strength 15.2 MPa
2200 psi
Typical
Garlock 7986 Neoprene Sheet Rubber
This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth cloth finishInformation provided by Garlock Rubber Technologies
Tensile Strength 15.2 MPa
2200 psi
ASTM D638
Saint-Gobain Rulon® 957 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation
Tygon S3â„¢ B-44-3, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-ba..
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Saint-Gobain Tygon® S3™ B-44-4X I.B. Pressure Tubing Formulation for filling, draining, transfer and processing applications
Tygon S3â„¢ B-44-X I.B. tubing, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products...
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Saint-Gobain Tygon® S3™ B-44-4X Phthalate-free Food, Milk, and Dairy tubing
Tygon S3â„¢ B-44-4X, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-b..
Tensile Strength 15.2 MPa
2200 psi
ASTM D412
Saint-Gobain Tygon® Transflow S3™ M-34-R Raw Milk Dairy Tubing Formulation
Transflow S3â„¢ M-34-R tubing, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. ..
Tensile Strength 15.2 MPa
2200 psi
AlphaGary Garaflex™ E 4362 A1 LCF Vinyl Thermoplastic Elastomer
Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cable 75°C rated low temperature booster cable jacket
Tensile Strength 15.2 MPa
2200 psi
AlphaGary Garaflex™ G 7789-A4 Thermoplastic Elastomer
Garaflex™ G is a thermoplastic elastomer intended for wire and cable applications105°C rated flexible jacket / insulation compound with excellent low temperature properties.
Tensile Strength 15.2 MPa
2200 psi
AlphaGary Garaflex™ O 9940 DWN-R Olefinic Thermoplastic Elastomer
Garaflex™ O is a flame retarded, olefinic thermoplastic elastomer125°C rated flame retardant olefinic TPE with excellent dry and wet electrical stability
Tensile Strength 15.2 MPa
2200 psi
AlphaGary Smokeguard™ LS III 1041 B Low Smoke Polyvinyl Chloride
Azoxymethane Free Low Cost Fiber Optic Jacket/Buffer Compound. Application example includes Optical Cables
Tensile Strength 15.2 MPa
2200 psi
AlphaGary GW 2280 M VW1 LCF Flame Retardant Polyvinyl Chloride
75°C or 80°C low temperature rated flexible jacketing compound intended for UL 62 application
Tensile Strength 15.2 MPa
2200 psi
AlphaGary Smokeguard™ LS III 1042 B Low Smoke Polyvinyl Chloride
Azoxymethane Free Low Cost Category Cable Jacket/Insulation