AlphaGary GW 3040 LT LCF Flame Retardant Polyvinyl Chloride

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer AlphaGary
Trade Name GW
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary GW 3040 LT LCF Flame Retardant Polyvinyl Chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
90°C rated jacket compound for riser applications with improved low temperature performance
Mechanical Properties Metric English Comments
Tensile Strength 15.9 MPa
2300 psi
Elongation at Break 270 %
270 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
Oxygen Index 40 %
40 %