Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AlphaGary Garaflex™ E 4832 Natural UV LCF Vinyl Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer AlphaGary
Trade Name Garaflex™ E
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garaflex™ E 4832 Natural UV LCF Vinyl Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cableA lead free, up resistant, flame retarded, oil resistant compound designed for wind turbine jacket applications
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 83
70 - 83
Tensile Strength 18.6 MPa
2700 psi
Elongation at Break 380 %
380 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -44.0 °C
-47.2 °F
Oxygen Index 32 %
32 %