Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 18.6 MPa | 2700 psi | ISO 527 |
S&E Specialty Polymers TufFill™ 5010UV Polyolefin Application: Thermoplastic polyolefin material is designed for automotive interior and exterior application. This product can be supplied in natural or an OEM matched color with UV protection or pai.. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-3174D PVC Compound Application: RoHS compliant, 60°C , general purpose PVC based compound suitable for extrusion applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 18.6 MPa | 2700 psi | Optimum; With provided formulation; ASTM D638 |
PolyOne Geon™ Specialty Suspension Atlas E 46 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas E 46 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for instan.. |
|||
Tensile Strength | 18.6 MPa @Strain 100 % |
2700 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3863 Polyvinyl Chloride, Flexible (PVC, Flexible) XV3863 is a flexible (95A durometer) vinyl compound formulated from FDA-santioned raw materials. XV3863 Clear 1859 has been tested to USP Class VI.NOTE: All ingredients used in the formulation of th.. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GM-94-106D PVC Compound Application: A clear, PVC based, extrusion grade compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | >= 18.6 MPa | >= 2700 psi | ASTM D 638 |
Karina E 90/212-DA-IS-SI-AT Compound PVC Crystal PVC Compound used for films. Non-toxic. Approved by food packaging safety, Pira International, United Kingdom.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 18.6 MPa | >= 2700 psi | ASTM D 638 |
Karina 937-48/1-CY-IS-BZ Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 18.6 MPa | >= 2700 psi | ASTM D 638 |
Karina E 85/253-IS-SI-AT Compound PVC Crystal Crystal/clear food grade PVC compound, recommended for cling films, specially developed for the European market.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | Average; ASTM D412 Method A |
Seals Eastern 7352D Nano-PTFE Filled Fluoroelastomer Nano-PTFE filled fluoroelastomer for low wear in hot dynamic applicationsInformation provided by Seals Eastern. |
|||
Tensile Strength | >= 18.6 MPa | >= 2700 psi | Qualified |
Shandong Dongyue Polymer DF-201 PTFE Fine Powder Usage: It is suitable for making unsintered tape.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE should be stored in a clean, dry warehouse.. |
|||
Tensile Strength | >= 18.6 MPa | >= 2700 psi | Qualified |
Shandong Dongyue Polymer DF-202 PTFE Fine Powder Usage: It is mainly used to process, belt, thin sheet and unsintered tape, thin wall rod etc.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTF.. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | ASTM D638 |
Ensinger Tecatron® XP-78 Compression Molded PPS Compound, 47% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | |
AlphaGary Smokeguard™ LS IV 1320 Low Smoke Polyvinyl Chloride Smokeguard™ IV 1320 is a high performance, lead free, low smoke PVC compound designed for demanding applications where PVDF would typically be used |
|||
Tensile Strength | 18.6 MPa | 2700 psi | ASTM D638 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | ASTM D638 |
Americas Styrenics STYRON A-TECH® 1260 High Impact Polystyrene Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa.. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | |
AlphaGary Garaflex™ E 4832 Natural UV LCF Vinyl Thermoplastic Elastomer Garaflex™ E is a vinyl based thermoplastic elastomer used mostly in wire and cableA lead free, up resistant, flame retarded, oil resistant compound designed for wind turbine jacket applications |
|||
Tensile Strength | 18.6 MPa | 2700 psi | |
AlphaGary GW 3003 LCF Q Flame Retardant Polyvinyl Chloride 80°C rated jacket compound |
|||
Tensile Strength | 18.6 MPa | 2700 psi | |
AlphaGary GW 3026 A LCF Flame Retardant Polyvinyl Chloride 75°C rated jacket compound intended for thin wall applications |
|||
Tensile Strength | 18.6 MPa | 2700 psi | |
AlphaGary GW 3026 LCF Flame Retardant Polyvinyl Chloride 60°C or 75°C rated jacket compound. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | |
AlphaGary GW 3028 LCF Flame Retardant Polyvinyl Chloride 60°C rated jacket compound. |
|||
Tensile Strength | 18.6 MPa | 2700 psi | ASTM D4894 |
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material Excellent heat, wear, and chemical resistance; Good cryogenic properties; Can be abrasive running against soft metals at high surface speed; Excellent material for back-up rings
Information .. |