Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

AlphaGary Garathane™ X 05-309 A3 Polyurethane based compound

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer AlphaGary
Trade Name Garathane™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Garathane™ X 05-309 A3 Polyurethane based compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Abrasion & Slip Resistant
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 54 - 62
54 - 62
Tensile Strength 10.3 MPa
1500 psi
Elongation at Break 400 %
400 %
Flex Crack Resistance 35000
35000
Ross Flex