AlphaGary PVC 2212/7-118 CLEAR 0003 Polyvinyl Chloride Thermoplastic

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded , PVC, Transparent
Manufacturer AlphaGary
Trade Name PVC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary PVC 2212/7-118 CLEAR 0003 Polyvinyl Chloride Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crystal clear, with high melt flow and excellent heat stability characteristics for connectors, drip chambers and accessories to medical bags and cathetersFormulated for injection molding or extrusion
Mechanical Properties Metric English Comments
Hardness, Shore D 79
79
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear; thickness not specified
Descriptive Properties Value Comments
DEHP Free No
Phthalate Free Yes