Material Notes:
Information provided by Spartech
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc

@Temperature 22.8 °C
1.01 g/cc

@Temperature 73.0 °F
ASTM D792
Filler Content 12 %
12 %
Mica
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
0.125inch wall
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
secant; ASTM D790
1.97 GPa
285 ksi
tangent; ASTM D790
Izod Impact, Notched 0.320 J/cm

@Temperature 22.8 °C
0.600 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C
135 °F
ASTM D648