Amco Amalloy® B1017A Clear Multipolymer Alloy

Category Polymer , Thermoplastic
Manufacturer Amco Plastic Materials
Trade Name Amalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco Amalloy® B1017A Clear Multipolymer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Amco Amalloy B1017A is a high impact multipolymer with exceptional clarity, good tensile and flexural strength, and medium-high melt flow.Super high impact, medium melt flow, good tensile and flexural strength.Information provided by Amco Plastic Materials.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.8 MPa
3300 psi
ASTM D638
Tensile Strength, Yield 24.8 MPa
3600 psi
ASTM D638
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
ASTM D256
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified