Polymer Property : Melt Flow = 5.0 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black
Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products.
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
PolyOne Maxxam™ PPR-20G Nat Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Plastcom SLOVAMID® 6 T 30 FRC 4 TS PA6 flame retarded, heat stabilized
PA 6 for injection molding, reinforced with 30% mineral filler, flame retarded with nonhalogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 3 at 1,6 mm, glo..
Melt Flow 5.0 - 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 - 10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..
Melt Flow 5.0 - 12 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 - 12 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized
Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Melt Flow 5.0 - 15 g/10 min

@Load 2.16 kg,
Temperature 250 °C
5.0 - 15 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage
Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen..
Melt Flow 5.0 - 9.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 - 9.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Ravago Manufacturing Americas Hylex® P1310G10 HB Polycarbonate, 10% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 260 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific)
ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system.
Melt Flow 5.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Ineos ABS Lustran® 1460, Injection Grade  (discontinued **)
Injection molding grade, increased heat and impact resistance, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acqui..
Melt Flow 5.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® LUX7630C PC COPOLYMER
Lexan* LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm..
Melt Flow 5.0 - 22 g/10 min
5.0 - 22 g/10 min
ASTM D1238
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade
ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a..
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
LTL Color Compounds ColorRxâ„¢ ABS-0502ARX Biocompatible, Antimicrobial ABS
A biocompatible, high gloss injection molding grade of ABS for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc.
Melt Flow 5.0 - 13 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 - 13 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Kraton® D1160 B (SIS) Linear Triblock Copolymer
Description: Kraton D1160 B is a clear linear triblock copolymer based on styrene and isoprene with bound styrene of 18.5% mass. It is supplied from South America in the physical form identified: Kr..
Melt Flow 5.0 - 15 g/10 min

@Load 2.16 kg,
Temperature 150 °C
5.0 - 15 g/10 min

@Load 4.76 lb,
Temperature 302 °F
Taiwan Sheen Soon Sheenthane® AH-620 TPU for Hotmelt Adhesive
Thermoplastic polyurethane elastomer for hard hotmelt adhesiveExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Melt flow may be customized. Used for hot melt adhes..
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Techmer ES HiFill FR® ABS FR UV
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc.
Melt Flow 5.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Novodur® E401 ABS
Novodur E401 is a high impact extrusion grade with good surface appearanceInformation provided by Styrolution
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Styron Pulse® 1310 ABS + Polycarbonate
PULSE® 1310 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing..
Melt Flow 5.0 g/10 min
5.0 g/10 min
Washington Penn H2GF3 Polypropylene, 30% Glass Fiber Reinforced
Homopolymer. Excellent heat aged physical properties.Applications: Under hood applications, battery trays, exercise equipmentData provided by Washington Penn Plastic Co., Inc.
Melt Flow 5.0 g/10 min

@Temperature 230 °C
5.0 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Formosa Plastics Formolene® 5144L Homopolymer Polypropylene
Homopolymer for Injection Molded Applications requiring Heat Resistance Formolene® 5144L is a highly isotactic, nucleated polypropylene homopolymer designed for consumer products and appliance appl..
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Silver Metallic 70153 Concentrate Based In LDPE
DescriptionPOLYBATCH® 70153 is a silver metallic color concentrate based in LDPE. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATC..
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Polyram RamOfin PPC371B73 Polypropylene, 73% Mineral Filled
73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind.
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
A. Schulman PP 3482-01 Polypropylene Nucleated Homopolymer Polypropylene
DescriptionPP 3482 is a nucleated homopolymer polypropylene with excellent heat resistance and stiffness properties.ApplicationThis product is for injection molded applications and is in compliance ..
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ELASTO UK Dryflex® 660300S SEBS Based Material, Semi-Filled Qualities, 30A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ELASTO UK Dryflex® 660500S SEBS Based Material, Semi-Filled Qualities, 50A Hardness, Natural
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
Melt Flow 5.0 g/10 min

@Load 2.17 kg,
Temperature 210 °C
5.0 g/10 min

@Load 4.78 lb,
Temperature 410 °F
ASTM D1238
AdvanSource Biomaterials ChronoFlex® C 55D Biodurable Medical Grade Polyurethane
ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome..
Melt Flow 5.0 g/10 min
5.0 g/10 min
3M Dyneon™ THV 505ESDZ Fluoroplastic Granules
Fluoroplastic THV is a flexible, fluoroplastic electrostatic dissipative compound composed of tetrafluoroethylene, hexafluoropropylene and vinylidene fluoride in the form of pellets.Information prov..
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Plastcom SLOVALEN PH 51 T 20 Polypropylene Homopolymer, 20% Mineral Filled
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application ..
Melt Flow 5.0 - 22 g/10 min
5.0 - 22 g/10 min
ASTM D1238
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238, ISO 1133
DuPont Elvax® CM3326 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® CM3326 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Specialty grades of Elvax® have the unusual combination of high vinyl acetate levels and low..