Material Notes:
Amco Amalloy B9941 is a clear performance copolymer with exceptional clarity and toughness.Good flexural and tensile strength.Information provided by Amco Plastic Materials.
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.5 MPa
3700 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D638
Flexural Strength 54.5 MPa
7900 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Optical Properties Metric English Comments
Haze 3.4 %

@Thickness 2.54 mm
3.4 %

@Thickness 0.100 in
ASTM D1003
Transmission, Visible 90 %

@Thickness 2.54 mm
90 %

@Thickness 0.100 in
ASTM D1003
Users viewing this material also viewed the following: