Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

American Polymers 370 Polystyrene, High Heat

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Heat Resistant Grade
Manufacturer American Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF American Polymers 370 Polystyrene, High Heat.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by American Polymers, Inc. A high heat polystyrene produced in pellet form. It has excellent strength and clarity as well as fast set-up properties. Used in the manufacture of toys, containers, housewares, and medical applications. Processing methods include blow molding, extrusion and injection molding.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D892
Melt Flow 2.0 g/10 min
2.0 g/10 min
Condition G; ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.7 MPa
7350 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.60 GPa
377 ksi
ASTM D638
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Annealed; ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525