Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® G151 ABS (Europe-Africa-Middle East) CYCOLAC G151 is a flame retardant grade of ´new technology´ CYCOLAC which has been especially formulated to minimise many of the problems often associated with the processing of traditiona.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML3042 PC (Europe-Africa-Middle East) LEXAN ML3042 offers an extremely low light transparency in combination with a very high reflection. This product is ideally suited for lighting reflectors. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp DBL14 PC (Europe-Africa-Middle East) Internally lubricated Polycarbonate compound, comtaining Glass Bead and PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min |
Polimeri Europa SINKRAL B260 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-04-09-25 Very high heat injection moulding grade with good impact resistance for this category of ABS. Main.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
PolyOne Lubri-Tech™ ATH-000/05M Acetal Homopolymer - 5% MoS2
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | |
Ineos ABS Lustran® H950 Very high heat resistance,,Property data per ISO test methods. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527 |
Grupo Repol Dinalon® B1V25 PA6 Unreinforced Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KA000M POM (Europe-Africa-Middle East) LNP* LUBRICOMP* KA000M is a compound based on Acetal Copolymer resin containg Aramide and Proprietary Lubricant. Added features include Internally Lubricated. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Tensile Modulus | 2.60 GPa @Thickness 4.00 mm |
377 ksi @Thickness 0.157 in |
Injection Molded; ISO 527-2/50 |
Styron EMERGEâ„¢ 7570 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7570 Advanced Resin is a high flow, ignition-resistant PC/ABS blend that contains now chlorinated or brominated additives. Its superior processing makes it ideal for in.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM-D790 |
Polyram RamTough PZ503 Polycarbonate, Flame Retardant Flame retardant polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP H 1040 TG Polypropylene, 20% Mineral Filled PP homopolymer 20% mineral fillerGood physical and mechanical characteristics, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 MR 309 HWCP Mineral Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1mm/min; ISO 527-1 |
Denka MALECCA K-090 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334T40L Talc Reinforced |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1mm/min; ISO 527 |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | 1mm/min; ISO 527 |
BASF Ultramid® A3HG2 10% Glass Filled PA66 (Conditioned) Ultramid A 3HG2 is a 10% glass fiber reinforced grade of nylon 6/6 for injection molding. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-1/-2 |
DSM Arnite® T06 200 SNF PBT (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Tensile Modulus | 2.60 GPa | 377 ksi | ISO 527-2 |
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an.. |