Ametek P410L P/M Stainless Steel, Sintered from 6.6 g/cc Green Density

Category Metal , Ferrous Metal , Stainless Steel , T 400 Series Stainless Steel
Manufacturer Ametek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ametek P410L P/M Stainless Steel, Sintered from 6.6 g/cc Green Density.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Powder apparent bulk density 2.8 g/cc; powder flow 30 sec/50g.Compacting properties measured on powders with 1% lithium stearite. Sintering was done in dissociated ammonia at 1121°C (2050°F) for 45 minutes. Sintered properties below were determined using transverse rupture bars. Compacting pressure 50 tsi. Green strength 2200 psi. Sintered breaking strength 120 ksi. Dimensional change from die size -0.24%.Information provided by Ametek Specialty Metal Products.
Physical Properties Metric English Comments
Density 6.67 g/cc
0.241 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 80
80
Tensile Strength, Ultimate 440 MPa
63800 psi
Elongation at Break 5.3 %
5.3 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 11.5 - 13.5 %
11.5 - 13.5 %
Iron, Fe 83.5 - 88.5 %
83.5 - 88.5 %
as balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %